DB6 Hot Die Steel
Comparable Standards
Designation | Standard |
DIN W.Nr. 1.2714 | DB6 |
AISI/SAE | DB6 |
Chemical Composition (wt %)
C | Si | Mn | P (max) | S (max) | Cr | Mo | V |
0.27–0.33 | 0.20–0.35 | 0.30–0.60 | 0.030 | 0.030 | 0.30 | 0.20 | 0.20 |
Mechanical Properties
Property | Value |
Typical Hardness | 50–55 HRC |
Tensile Strength | 900 MPa |
Heat Treatment Guidelines
– Annealing: 650–680 °C; furnace cool
– Hardening: 800–820 °C; oil quench
– Tempering: 550–570 °C; 2× cycles
Typical Applications
– Plastic mould cores
– Mould cavities
– High-wear mould components
Supply Formats & Services
– Stocked Shapes: Rounds (20 – 350 mm Ø), Flats (25 × 50 – 200 × 500 mm), Blocks (up to 2,000 kg)
– Custom Cutting: Precision bandsaw to drawing
– Value-Added Services: In-house forging & heat treatment, Ultrasonic (UT) & MPI testing, Hardness & microstructure analysis, Pre-machining & surface grinding
Certifications & Quality Assurance
– Mill-Traceable Test Certificates (EN 10204 3.1)
– Ultrasonic & MPI Reports (ASTM A388 on request)
– Hardness, Grain-Size & Decarb Analysis
– ISO 9001:2015 (certification in process)
Logistics & Enquiry
– Same-day Dispatch for stocked items from Kolkata
– 24–48 hr turnaround on custom-cut materials
– PAN-India Delivery via trusted logistics partners